Pengaruh Penambahan Aditif Sikament-Ln terhadap Kuat Tekan Beton Mutu Tinggi dengan Variasi Nilai Slump
Abstract
High-strength concrete listed in SNI 03-6468-2000 concrete is defined as concrete having the required compressive strength of fc'≥ 41 Mpa. From this study, data obtained from the compressive strength of concrete at the age of 28 days as follows: the value of the normal concrete compressive strength of 41.72 MPa, the compressive strength of the Sikament-ln mixture of 0.6% slump 5 of 45.65 MPa, the compressive strength of the Sikament-mixed concrete. -ln 1% slump 6 of 47,38 MPa, compressive strength of mixed concrete Sikament-ln 1.4% slump 7 of 44.20 MPa, compressive strength of mixed concrete of Sikament-ln 1.8% slump 8 of 45.65 MPa 38 ,65MPa. It can be seen from the results of this study that the ideal compressive strength is the compressive strength of the Sikament-ln mixture of 1% slump 6 this is because the compressive strength value is much greater than the compressive strength without the Sikament-ln mixture.
Keywords
Full Text:
PDFReferences
Arman, A, 2019. Study Eksperimen Pengaruh Campuran Sika LN dalam Meningkatkan Kuat Tekan Bata Beton Ringan, Jurnal Menara Ilmu Vol. 13, No.1.
Andika, Y., & Bida Rehi, N. 2020. Pengaruh Waktu Pencampuran terhdap Kuat Tekan Cmapuran Beton Dengan Bahan Tambah Sikament-LN. Jurnal Karkasa, Vol. 6, No. 1.
Dapas Servie O, Sumajouw Marthin D.J. 2020, Studi Eksperimental Pengujian Kuat Tekan Beton Menggunakan Kapur dan Batu Apung Sebagai Bahan Pengganti Sebagaian Semen, Jurnal Sipil Statik, Vol.8 No.5.
Hadidi, Chrisna Djaja Mungokk. 2013. Studi Eksperimental Pemakaian High Range Water Reducing dengan Sikament LN Terhadap Beton Mutu Normal Menggunakan Metode ACI. Jurnal Mahasiswa Teknik Sipil Universitas Tanjung Pura, Vol.1, No.1.
Rahmat, Hendriyani Irna, Anwar Moh. Syaiful, 2016. Analisis Kuat Tekan Beton dengan Bahan Tambahan Reduced Water dan Accelerated Admixture, Jurnal Info Teknik Vol. 17, No.2.
SNI 03-1972-1990. Metode Pengujian Slump Beton. ICS. Bandung.
SNI 15-2049-2004. Semen Portland. Badan Standarisasi Nasional. Bandung.
SNI 1972-2008 Tentang Cara Uji Slump Beton. Badan Standarisasi Nasional, Jakarta.
SNI PD-T-04-2004-C. Tata Cara Pembuatan dan Pelaksanaan Beton Berkekuatan Tinggi. Departemen Pemukiman dan Prasarana Wilayah.
Tjokrodimuljo, Kardiyono, 1996. Teknologi Beton, Penerbit Nafiri, Yogyajarta.
DOI: http://dx.doi.org/10.33087/talentasipil.v6i2.332
Refbacks
- There are currently no refbacks.

This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.
Jurnal Talenta Sipil, Faculty of Engineering, Batanghari University |